Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of Kynar Flex® PPA 8600 - PVDF - ARKEMA
unit conversion, PDF datasheet print, comparison with other plastics
Check here, which other Kynar Flex datasheets, application examples or technical articles are available in Material Data Center
Kynar Flex® PPA 8600 resin is specially designed pellet used as a polymer process aid (PPA) for polyolefins.
The use of Kynar Flex® PPA 8600 resin at 200 - 1000 ppm levels reduces extruder pressure, improves surface finish, reduces die build up, and improves gauge control.
This product is also available on a powder form as Kynar Flex® PPA 8601 resin.
Proprietà Termiche | Valore | Unitá | Norma del test | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ISO Data | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Temperatura di fusione, 10°C/min | 165 | °C | ISO 11357-1/-3 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Temperatura di transizione vetrosa, 10°C/min | -40 | °C | ISO 11357-1/-2 |
Altre Proprietà | Valore | Unitá | Norma del test |
Massa volumica | 700 | kg/m³ | ISO 1183 |